Patents with Abstracts

8,188,169 
Polyoxymethylene compositions and articles made from these
 
Moraczewski and Pollino of DuPont, Delaware, developed polyoxymethylene compositions that include 90 to 99.9 wt% of at least one polyacetal polymer and 0.1 to 10 wt % of at least one polysaccharide substantially free of acidic material selected from the group consisting of amylopectin from maize and soluble starch. (RDC 6/7/2012)

8,178,627 
Oxymethylene copolymer composition for stretching material, stretching material, structures, and process for producing the same
 
Okamura of Mitsubishi, Japan, developed an oxymethylene copolymer material for a stretched material having a high strength and a high elastic modulus.  This material consists of an oxymethylene copolymer; and a crosslinkable compound to be blended with 0.001 to .05 phr oxymethylene copolymer. The present invention also relates to a stretched material obtained by using the oxymethylene copolymer composition. Further, the present invention relates to a structure obtained by the secondary processing of the above stretched material, and a structure obtained by using the above oxymethylene copolymer composition in a bonding layer of the structure. The present invention also relates to a method of producing a structure, the method including: using the oxymethylene copolymer composition in a bonding layer of the structure; and removing a polyalkylene glycol component with water or a solvent. (RDC 5/29/2012)

8,138,247 
Polyoxymethylene compositions and articles made from these
 
Shinohara and Shibuya  of DuPont, Delaware, developed a polyoxymethylene material consisting of (a) 20 to 80 wt% polyacetal homopolymer, copolymer, or mixtures of these; (b) 5 to 40 wt% glass fiber; (c) 0.1 to 2 wt% polymeric thermal stabilizer selected from the group consisting of polyacrylamide, polymethacrylamide, and mixtures of these; (d) 0.02 to 2 wt% allantoin; and 0.1 to 5 wt% of an ethylene copolymer of the formula E/X/Y; wherein Y includes a glycidyl group (RDC 5/16/2012)

xxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxx 

Roger D. Corneliussen
Editor
www.maropolymeronline.com

Maro Polymer Links
Tel: 610 363 9920
Fax: 610 363 9921
E-Mail: cornelrd@bee.net  

***********************************

Copyright 2012 by Roger D. Corneliussen.
No part of this transmission is to be duplicated in any manner or forwarded by electronic mail without the express written permission of Roger D. Corneliussen
**************************************

** Date of latest addition; date of first entry is 5/16/2012.